Cold rolled steel is produced by further processing hot rolled steel through cold reduction mills (at room temperature) followed by annealing and/or temper rolling to produce steel with closer dimensional tolerances and a wider range of surface finishes.

QualityRelevant SpecificationsCharacteristics
Carbon – ManganeseA1008 CSGood Formability, Mechanical Properties not specified.
Commercial SteelType A, B, C
Drawing SteelA1008 DSNon Aging Steel, minimizes possible fluting and stretcher strains during forming.
Type A, B
Deep Drawing SteelA1008 DDS
Extra Deep Drawing SteelA1008 EDDS
Structural SteelA1008 SS(various strength levels) minimum yield strength ranging from 25,000 PSI to 80,000 PSISpecified whenever guaranteed mechanical properties are required.

THEORETICAL WEIGHT PER SQUARE FOOT 
COLD ROLLED (.135–.0149)

GaugeNominal Thickness In InchesEstimated Weight Per Square Foot
70.17937.5
80.16446.875
90.14956.25
100.13445.625
110.11965
120.10464.375
130.08973.75
140.07473.125
160.05982.5
180.04782
200.03591.5
220.02991.25
240.02391
260.01790.75
280.01490.625